Hi

I am trying to deposit about 5.0 um thick Aluminum film on 20um
photoresist/polymer. But the metal layer does not adhere well on
photoresist/polymer and peels off. Some of the methods I have tried to improve
the adhesion are degas, preclean, Ti glue layer etc. Because of the photoresist,
I can not increase the substrate temp more than 150C. Has any one come across
this kind of problem and possible solution?

With regards,

Pramod

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMS Technology Review