A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: removal of HMDS without affecting the photoresist
removal of HMDS without affecting the photoresist
2010-10-20
Mikael Evander
2010-10-21
Jesse D Fowler
2010-10-21
Gareth Jenkins
2010-10-21
David Casale
2010-10-22
Mikael Evander
2010-10-21
Shay Kaplan
2010-10-21
Bill Flounders
2010-10-26
Bill Moffat
removal of HMDS without affecting the photoresist
Bill Moffat
2010-10-26
Agree with Bill Flounders.  The 5 angstrom monolayer created by the HMDS
reaction is removed by any reasonably harsh organic remover.  Oxygen
plasma, Piranha, sulphuric acid and or sulphonic acids.

Bill
Yield Engineering Systems.

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On
Behalf Of Bill Flounders
Sent: Thursday, October 21, 2010 9:03 AM
To: General MEMS discussion
Cc: Shay Kaplan
Subject: Re: [mems-talk] removal of HMDS without affecting the
photoresist

After developing the photoresist, a brief O2 plasma treatment will
remove any residual HMDS if there is even any remaining after
development.

The best tests to verify these effects would be to measure contact angle
of your surface prior to HMDS coat, after HMDS coat, then PR coat, flood
expose, develop - then test contact angle again.
Brief O2 plasma and test contact angle one more time.

This should give you all the info you need to verify your process.

I expect Bill Moffatt at Yield Engineering may weigh in on this also.

Sincerely,
Bill Flounders
Berkeley NanoLab
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMStaff Inc.