A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RE: 3" 7740 Glass
RE: 3" 7740 Glass
2000-02-28
[email protected]
RE: 3" 7740 Glass
[email protected]
2000-02-28
Sensor Prep Services, in Elburn Illinois, provides a good quality 7740
substrate. Contact them at (630) 365-9645 or email [email protected].
Specialty Glass also can provide glass substrates. They're in Willow Grove,
PA at (215) 659-8400
Good luck!
-Rich
Rich Hjulstrom
Siemens-Moore
Spring House, PA 19477

-----Original Message-----
From: Lyle Leverich [mailto:[email protected]]
Sent: Tuesday, February 22, 2000 6:20 PM
To: [email protected]
Subject: 3" 7740 Glass


Does anyone know a source for 3" 7740 or "Borofloat" wafers ?


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Harrick Plasma, Inc.