Hello,

I have an adhesion problem between Su-8 (development finished) and metal
layers. Actually, I'd like to make metal thin film structures on top of Su-8
using a lift off process. However, while removing PR ultrasonically in
acetone right after sputtering metal layers on top of Su-8, I found that not
only PR but also the metal layers came off. Does anyone know how to make
metal layers stick to the Su-8? Cr/Au is used as metal layer and the Su-8 is
completely processed (pre-baking, exposure, PEB, development).

Thanks in advance.

Best,
Sungdong Kim
==============================
Sungdong Kim
ISTG, MESA+ Research Institute
University of Twente
P.O.Box 217
7500 AE Enschede
The Netherlands
Phone: +31-53-4892747
Fax: +31-53-4893343
E-mail: [email protected] 
==============================


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing