1996-02-26
Aylin
Silicon Etching
Aylin
1996-02-26
After having dissolved eleven silicon wafers (77g) in the same KOH/H2O solution
we could suddenly watch some complexes forming. They are black and even
soluable in water.

Did you ever see the same, have you got an idea what could it be? I think they
are bondings between potassium and silicondioxid built at a certain
concentration of silicon in the solution. Any ideas concerning the chemistry?


Aylin

**************************************************************************
Aylin Hein, Technical University Berlin, Microsensor & Actuator Technology
Email:  [email protected]
URL:    http://www-mat.ee.tu-berlin.de/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
The Branford Group
Addison Engineering