Material: Aluminum (Al), bulk

To purchase MEMS-related materials, supplies, equipment, wafers, etc.,please visit the links section of the MEMSNet site.

Property↑↓Value↑↓Conditions↑↓Reference↑↓
Density2700 kg/m^3Solid DensityCRC Materials Science and Engineering Handbook, p.46
Specific heat898.7 J/kg/KAt Temp=25 C.CRC Materials Science and Engineering Handbook, p.260
Thermal conductivity237 W/m/KValue at temp=300 K.CRC Materials Science and Engineering Handbook, p.270-274
Young's Modulus70 GPaBulk material.Thin Solid Films,270(1995), p.263