Property↑↓Value↑↓Conditions↑↓Reference↑↓
Density5600 kg/m^3CeramicCRC Materials Science and Engineering Handbook, p.50
Electrical resistivity210000 Ω*mCeramicCRC Materials Science and Engineering Handbook, p.563
Hardness,Knoop(KH)1700 kg/mm/mmCeramic,100gCRC Materials Science and Engineering Handbook, p.470
Hardness,Micro1800 kg/mm/mmCeramic,100gCRC Materials Science and Engineering Handbook, p.470
Hardness,Vickers(VH)1800 kg/mm/mmCeramic,50gCRC Materials Science and Engineering Handbook, p.470
Tensile strength0.731 GPaCeramicCRC Materials Science and Engineering Handbook, p.405
Thermal conductivity20.48 .. 31.77 W/m/KAt room temperature.CRC Materials Science and Engineering Handbook, p.278
Young's Modulus211.04 GPaCeramicCRC Materials Science and Engineering Handbook, p.507