Property↑↓Value↑↓Conditions↑↓Reference↑↓
Specific heat518.32 J/kg/KAt Temp=25 C.CRC Materials Science and Engineering Handbook, p.260
Young's Modulus1143 GPa(density=3512 kg/m/m/m),Obtained from SAW technique, using the ns Nd:YAG at 355 nm for launching and the probe beam deflection arrangement for detecting the SAW pulses.Applied Surface Science 106(1996), p.434