Material: Diamond (C), film

To purchase MEMS-related materials, supplies, equipment, wafers, etc.,please visit the links section of the MEMSNet site.

Property↑↓Value↑↓Conditions↑↓Reference↑↓
Young's Modulus940 GPa(density=3450 kg/m/m/m), Obtained from SAW technique ,using the ns Nd:YAG at 355 nm for launching and the probe beam deflection arrangement for detecting the SAW pulses.Applied Surface Science 106(1996), p.434
Young's Modulus1040 GPa(density=3510 kg/m/m/m), Obtained from SAW technique ,using the ns Nd:YAG at 355 nm for launching and the probe beam deflection arrangement for detecting the SAW pulses.Applied Surface Science 106(1996), p.434
Young's Modulus800 .. 1140 GPaCVD film,obtained from laser induced ultrasonic surface wave method for a thickness of 2-13 um.Thin Solid Films 290-291(1996), p.309