Material: Iron (Fe), bulk

To purchase MEMS-related materials, supplies, equipment, wafers, etc.,please visit the links section of the MEMSNet site.

Property↑↓Value↑↓Conditions↑↓Reference↑↓
Density7800 kg/m^3Single crystal.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Hardness,Knoop(KH)400 kg/mm/mmSingle crystal.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Thermal conductivity80.3 W/m/KSingle crystal.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Yield strength12.6 GPaSingle crystal.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Young's Modulus196 GPaSingle crystal.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421