Material: Lead Zirconate Titanate (PZT)

To purchase MEMS-related materials, supplies, equipment, wafers, etc.,please visit the links section of the MEMSNet site.

Property↑↓Value↑↓Conditions↑↓Reference↑↓
Coupling coefficient,k310.35Piezoelectric bimorph G-1195,Two layer,thickness of each layer=0.0075 inch,central shim=0.005 inch stainless steel, Curie temp=360 C.J.MEMS,DEC 1995,Vol.4,NO.4, p.234
Coupling coefficient,k330.69Piezoelectric bimorph G-1195,Two layer,thickness of each layer=0.0075 inch central shim=0.005 inch stainless steel,Curie temp=360 C,J.MEMS,DEC 1995,Vol.4,NO.4, p.234
Density7500 kg/m^3Piezoelectric material,used in Piezoelectric actuators.IEEE 5th International Symposium on Micro Machine and Human Science proceedings,Nagoya, Oct 1994, p.75
Density7600 kg/m^3Piezoelectric bimorph G-1195,Two layer,thickness of each layer=0.0075 inch central shim=0.005 inch stainless steel,Curie temp=360 C,J.MEMS,DEC 1995,Vol.4,NO.4, p.234
Density7600 kg/m^3Piezoelectric bimorph G-1195,Two layer,thickness of each layer=0.0075 inch,central shim=0.005 inch stainless steel, Curie temp=360 C.J.MEMS,DEC 1995,Vol.4,NO.4, p.234
Dielectric constant,relative,K11700Piezoelectric bimorph G-1195,Two layer,thickness of each layer=0.0075 inch,central shim=0.005 inch stainless steel, Curie temp=360 C.J.MEMS,DEC 1995,Vol.4,NO.4, p.234
Dielectric constant,relative,K3&K11700Piezoelectric bimorph G-1195,Two layer,thickness of each layer=0.0075 inch central shim=0.005 inch stainless steel,Curie temp=360 C,J.MEMS,DEC 1995,Vol.4,NO.4, p.234
Strain coefficient(Piezoelectric),d311.8e-10 m/VPiezoelectric bimorph G-1195,Two layer,thickness of each layer=0.0075 inch,central shim=0.005 inch stainless steel, Curie temp=360 C.J.MEMS,DEC 1995,Vol.4,NO.4, p.234
Strain coefficient(Piezoelectric),d333.6e-10 m/VPiezoelectric bimorph G-1195,Two layer,thickness of each layer=0.0075 inch central shim=0.005 inch stainless steel,Curie temp=360 C,J.MEMS,DEC 1995,Vol.4,NO.4, p.234
Strain constant(piezoelectric)1.1e-10 m/VPiezoelectric material,used in Piezoelectric actuators.IEEE 5th International Symposium on Micro Machine and Human Science proceedings,Nagoya, Oct 1994, p.75
Voltage coefficient(Piezoelectric),g310.011 V*m/NPiezoelectric bimorph G-1195,Two layer,thickness of each layer=0.0075 inch,central shim=0.005 inch stainless steel, Curie temp=360 C.J.MEMS,DEC 1995,Vol.4,NO.4, p.234
Voltage coefficient(Piezoelectric),g330.025 V*m/NPiezoelectric bimorph G-1195,Two layer,thickness of each layer=0.0075 inch central shim=0.005 inch stainless steel,Curie temp=360 C,J.MEMS,DEC 1995,Vol.4,NO.4, p.234
Young's Modulus63 GPaPiezoelectric material,used in Piezoelectric actuators.IEEE 5th International Symposium on Micro Machine and Human Science proceedings,Nagoya, Oct 1994, p.75
Young's Modulus,Y1163 GPaPiezoelectric bimorph G-1195,Two layer,thickness of each layer=0.0075 inch,central shim=0.005 inch stainless steel, Curie temp=360 C.J.MEMS,DEC 1995,Vol.4,NO.4, p.234
Young's Modulus,Y3349 GPaPiezoelectric bimorph G-1195,Two layer,thickness of each layer=0.0075 inch central shim=0.005 inch stainless steel,Curie temp=360 C,J.MEMS,DEC 1995,Vol.4,NO.4, p.234