Property↑↓Value↑↓Conditions↑↓Reference↑↓
Specific heat756.58 J/kg/Kwhite,value measured at temp=25 C.CRC Materials Science and Engineering Handbook, p.260
Specific heat668.8 J/kg/KRed,triclinic ,value measured at temp=25 C.CRC Materials Science and Engineering Handbook, p.260