Property↑↓Value↑↓Conditions↑↓Reference↑↓
Density7400 kg/m^3Used in piezoelectric drivivg force actuator with 0.2 mm thickness.IEEE 5th International Symposium on Micro Machine and Human Science Proceedings,Nagoya,oct 1994, p.48
Dielectric constant,relative2000Used in piezoelectric drivivg force actuator with 0.2 mm thickness.IEEE 5th International Symposium on Micro Machine and Human Science Proceedings,Nagoya,oct 1994, p.48
Piezoelectric constant-1.95e-10 m/VUsed in piezoelectric drivivg force actuator with 0.2 mm thickness.IEEE 5th International Symposium on Micro Machine and Human Science Proceedings,Nagoya,oct 1994, p.48
Poisson's Ratio0.35Used in piezoelectric drivivg force actuator with 0.2 mm thickness.IEEE 5th International Symposium on Micro Machine and Human Science Proceedings,Nagoya,oct 1994, p.48
Stiffness58 GPaUsed in piezoelectric drivivg force actuator with 0.2 mm thickness.IEEE 5th International Symposium on Micro Machine and Human Science Proceedings,Nagoya,oct 1994, p.48