Property↑↓Value↑↓Conditions↑↓Reference↑↓
Density1780 kg/m^3Polymer,Thickness of 100 um, used in Piezoelectric actuatorsIEEE 5th International Symposium on Micro Machine and Human Science proceedings,Nagoya, Oct 1994, p.75
Strain constant(piezoelectric)2.3e-11 m/VPolymer,Thickness of 100 um, used in Piezoelectric actuatorsIEEE 5th International Symposium on Micro Machine and Human Science proceedings,Nagoya, Oct 1994, p.75
Young's Modulus2 GPaPolymer,Thickness of 100 um, used in Piezoelectric actuatorsIEEE 5th International Symposium on Micro Machine and Human Science proceedings,Nagoya, Oct 1994, p.75