Density7900 kg/m^3Used in silicon integrated circuits.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Hardness,Knoop(KH)660 kg/mm/mmUsed in silicon integrated circuits.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Thermal conductivity32.9 W/m/KUsed in silicon integrated circuits.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Yield strength2.1 GPaUsed in silicon integrated circuits.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Young's Modulus200 GPaUsed in silicon integrated circuits.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421