Property↑↓Value↑↓Conditions↑↓Reference↑↓
Poisson's Ratio0.3Material property used in the finite element computations of ultra microhardness indentation of thin films,both coating and substrate are assumed to be homogenous and elastic/plastic.Thin solid films 290-291(1996), p.363
Yield stress,equivalent400 MPaProperty used in the finite element computations of ultra microhardness indentation of thin films.Thin Solid Films 290-291(1996), p.363
Young's Modulus240 GPaMaterial property used in the finite element computations of ultra microhardness indentation of thin films,both coating and substrate are assumed to be homogeneous and elastic/plastic.Thin solid films 290-291(1996), p.363