Material: Titanium Carbide (TiC), Bulk

To purchase MEMS-related materials, supplies, equipment, wafers, etc.,please visit the links section of the MEMSNet site.

Property↑↓Value↑↓Conditions↑↓Reference↑↓
Density4900 kg/m^3Single crystal.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Density4920 .. 4938 kg/m^3CeramicCRC Materials Science and Engineering Handbook, p.50
Electrical resistivity0.003 .. 0.008 Ω*mCeramic,at temp=20 CCRC Materials Science and Engineering Handbook, p.564
Hardness,Knoop(KH)2470 kg/mm/mmSingle crystal.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Hardness,Knoop(KH)2470 kg/mm/mm100g,Ceramic.CRC Materials Science and Engineering Handbook, p.471
Hardness,Knoop(KH)1905 kg/mm/mm1000g,CeramicCRC Materials Science and Engineering Handbook, p.471
Hardness,Micro3200 kg/mm/mm20g,CeramicCRC Materials Science and Engineering Handbook, p.471
Hardness,Vickers(VH)2900 .. 3200 kg/mm/mm50g,CeramicCRC Materials Science and Engineering Handbook, p.471
Hardness,Vickers(VH)2850 .. 3390 kg/mm/mm100g,CeramicCRC Materials Science and Engineering Handbook, p.471
Heat capacity710.6 .. 781.66 J/kgCeramic,at temp=300 C.CRC Materials Science and Engineering Handbook, p.263
Heat capacity764.94 .. 819.28 J/kgCeramic,at temp=450 C.CRC Materials Science and Engineering Handbook, p.263
Heat capacity802.56 .. 840.18 J/kgCeramic,at temp=600 C.CRC Materials Science and Engineering Handbook, p.263
Heat capacity836 .. 865.26 J/kgCeramic,at temp=750 C.CRC Materials Science and Engineering Handbook, p.263
Heat capacity877.8 J/kgCeramic,at temp=1000 C.CRC Materials Science and Engineering Handbook, p.263
Heat capacity881.98 J/kgCeramic,at temp=1100 C.CRC Materials Science and Engineering Handbook, p.263
Heat capacity873.62 J/kgCeramic,at temp=900 C.CRC Materials Science and Engineering Handbook, p.263
Modulus of Rupture0.2253 GPaCeramic,density=4850 kg/m/m/m,at room temperatureCRC Materials Science and Engineering Handbook, p.532
Modulus of Rupture0.2253 GPaCeramic,density=4850 kg/m/m/m,at room temperatureCRC Materials Science and Engineering Handbook, p.532
Modulus of Rupture0.09379 GPaCeramic,density=4850 kg/m/m/m,at temp=2000 CCRC Materials Science and Engineering Handbook, p.532
Poisson's Ratio0.187 .. 0.189CeramicCRC Materials Science and Engineering Handbook, p.537
Tensile strength0.1186 GPaCeramic,at temp=1000 CCRC Materials Science and Engineering Handbook, p.405
Thermal conductivity330 W/m/KSingle crystal.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Thermal conductivity17.14 .. 30.93 W/m/KCeramic,at room temperature.CRC Materials Science and Engineering Handbook, p.279
Thermal conductivity5.64 W/m/KCeramic,at Temp=1000 C.CRC Materials Science and Engineering Handbook, p.279
Yield strength20 GPaSingle crystal.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Young's Modulus497 GPaSingle crystal.Proceedings of IEEE,Vol 70,No.5,May 1982, p.421
Young's Modulus439.43 GPaCeramic,at room temperatureCRC Materials Science and Engineering Handbook, p.508
Young's Modulus310.34 .. 379.31 GPaCeramic,at temp=1000 CCRC Materials Science and Engineering Handbook, p.508