Material: Tool steel

To purchase MEMS-related materials, supplies, equipment, wafers, etc.,please visit the links section of the MEMSNet site.

Property↑↓Value↑↓Conditions↑↓Reference↑↓
Density7900 kg/m^3Contact pin ,used in pin-type piezoelectric driving force actuators,model-A,B,C,D.IEEE 5th International Symposium on Micro Machine and Human Science proceedings,Nagoya, Oct 1994, p.48
Poisson's Ratio0.29Contact pin ,used in pin-type piezoelectric driving force actuators,model-A,B,C,D.IEEE 5th International Symposium on Micro Machine and Human Science proceedings,Nagoya, Oct 1994, p.48
Young's Modulus210 GPaContact pin ,used in pin-type piezoelectric driving force actuators,model-A,B,C,D.IEEE 5th International Symposium on Micro Machine and Human Science proceedings,Nagoya, Oct 1994, p.48