Material: Tungsten Silicide (WSi2), bulk

To purchase MEMS-related materials, supplies, equipment, wafers, etc.,please visit the links section of the MEMSNet site.

Property↑↓Value↑↓Conditions↑↓Reference↑↓
Density9250 .. 9300 kg/m^3CeramicCRC Materials Science and Engineering Handbook, p.52
Electrical resistivity33.4 .. 549000 Ω*mCeramicCRC Materials Science and Engineering Handbook, p.567
Hardness,Knoop(KH)1090 kg/mm/mm100g,CeramicCRC Materials Science and Engineering Handbook , p.475
Hardness,Micro1260 kg/mm/mm50g,CeramicCRC Materials Science and Engineering Handbook, p.475
Hardness,Vickers(VH)1090 kg/mm/mm100g,CeramicCRC Materials Science and Engineering Handbook, p.475
Hardness,Vickers(VH)1632 kg/mm/mm10g,CeramicCRC Materials Science and Engineering Handbook, p.475
Heat capacity33440 J/kg/KAt temp=425-1450 C.CRC Materials Science and Engineering Handbook, p.263