Material: Zirconium Oxide (ZrO2),

To purchase MEMS-related materials, supplies, equipment, wafers, etc.,please visit the links section of the MEMSNet site.

Property↑↓Value↑↓Conditions↑↓Reference↑↓
Young's Modulus171.03 .. 186.21 GPaCeramic,at room temperatureCRC Materials Science and Engineering Handbook, p.511
Young's Modulus248.28 GPaCeramic,at temp=20 CCRC Materials Science and Engineering Handbook, p.511
Young's Modulus13.793 GPaCeramic,at temp=500 CCRC Materials Science and Engineering Handbook, p.511
Young's Modulus130.37 GPaCeramic,at temp=800 CCRC Materials Science and Engineering Handbook, p.511
Young's Modulus127.61 .. 172.41 GPaCeramic,at temp=1000 CCRC Materials Science and Engineering Handbook, p.511
Young's Modulus127.61 .. 172.41 GPaCeramic,at temp=1000 CCRC Materials Science and Engineering Handbook, p.511
Young's Modulus21.023 GPaCeramic,at temp=1100 CCRC Materials Science and Engineering Handbook, p.511
Young's Modulus117.91 .. 124.13 GPaCeramic,at temp=1200 CCRC Materials Science and Engineering Handbook, p.511
Young's Modulus97.931 GPaCeramic,at temp=1400 CCRC Materials Science and Engineering Handbook, p.511
Young's Modulus88.276 GPaCermic,at temp=1500 CCRC Materials Science and Engineering Handbook, p.511