MEMSnet Home: MEMS-Talk: Re: Fix Fibre in Groove (using UV curing glue, from Xuming Zhang)
Re: Fix Fibre in Groove (using UV curing glue, from Xuming Zhang)
2003-04-26
Zhang Xuming
Re: Fix Fibre in Groove (using UV curing glue, from Xuming Zhang)
Zhang Xuming
2003-04-26
Dear Jun Yao:

Summary: Using UV curing glue to package fibers to grooves/substrate.

A typcial and professional solution for fiber attachment to grooves/substrates
is using UV curing glue (or resin). Steps: (1) align the fibers to their desired
positions; (2) apply some UV curing glue to the fibers by use of a air-
controlled dispensor; (3) Use UV light source to shine and cure the glue.

Beste Regards,

Zhang Xuming  Simon
Nanyang Technological University (NTU), Singapore
Tel: (65) 6790 5461   Fax: (65) 6790 4161

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.