Re: Cheap Resist Spinner...
2003-05-08
Edwin Jager
Re: Cheap Resist Spinner...
Edwin Jager
2003-05-08
I can recommend APT Polos spinner. Cheap and easy in use. You can contact
Bert van Weelde at SPS Europe. ([email protected])

Edwin

At 07:56 2003-05-08 -0400, you wrote:
>Message: 5
>Date: Wed, 7 May 2003 18:26:23 +0300
>From: "Sampo Tuukkanen" 
>Subject: [mems-talk] Cheap Resist Spinner...
>To: "MemsTalk" 
>Message-ID: <[email protected]>
>Content-Type: text/plain;       charset="iso-8859-1"
>
>Hi!
>
>I just broke our fotoresist spinner and...Ok, it was broken when I went to
>clean room...
>
>Does anyone know, where I could supply relatively cheap manual R&D resist
>spinner?
>It can be second-hand or new.
>
>- Sampo Tuukkanen
>
>_______________________________________________________
>Sampo Tuukkanen, Room K215, Department of Physics,
>PB 35 (YFL), FIN-40014 University of Jyväskylä, FINLAND
>E-mail: [email protected]
>Tel: +35814 260 2392, Fax: +358 14 260 2351

dr. ir. Edwin Jager
CTO                                             phone: +46-13-131650
Micromuscle AB                           GSM:  +46-733-601490
Westmansgatan 29                        fax: +46-13-131653
582 16  Linköping                             email:
[email protected]
Sweden                                         http://www.micromuscle.com



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMS Technology Review