Hello,
there is Riston from Dupont:
http://www.dupont.com/pcm/product.html
or Ordyl from elgaeurope
http://www.elgaeurope.it/
Regards,
Roland

At 12:00 08/05/2003 -0400, you wrote:
>Send MEMS-talk mailing list submissions to
>         [email protected]
>
>To subscribe or unsubscribe via the World Wide Web, visit
>         http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>or, via email, send a message with subject or body 'help' to
>         [email protected]
>
>You can reach the person managing the list at
>         [email protected]
>
>When replying, please edit your Subject line so it is more specific
>than "Re: Contents of MEMS-talk digest..."
>
>
>Today's Topics:
>
>    1. Dry film resist (Abdur Rub Abdur Rahman)
>
>
>----------------------------------------------------------------------
>
>Message: 1
>Date: Wed, 7 May 2003 23:43:36 -0400 (EDT)
>From: Abdur Rub Abdur Rahman 
>Subject: [mems-talk] Dry film resist
>To: [email protected]
>Message-ID: <[email protected]>
>Content-Type: text/plain
>
>I am looking to purchase dry film photoresist for some
>of my applications. can someone suggest some vendors
>and process tips.
>Thank you.
>
>
>Regards,
>Abdur
>
>
>------------------------------


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
The Branford Group