Ideas for alternative O-Rings
2003-05-08
Maurice Norcott
2003-05-09
R. Brent Garber (2 parts)
Ideas for alternative O-Rings
Maurice Norcott
2003-05-08
I need to find a substitute for viton o-rings. It's a room temperature
application that needs to pull a light vacuum while being very compressive
(soft and pliable). The x-section profile can be square or round. Any
suggestions appreciated.



Maurice H. Norcott
Senior Technician
Silicon Genesis Corporation
61 Dagget Drive
San Jose, CA 95134-2109

408-228-5852 Office
408-977-6333 Pager
408-228-5908 Lab
408-432-3832 FAX
[email protected]



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation
University Wafer