MEMSnet Home: MEMS-Talk: Re: Al / 2% / Si MEMS-talk Digest, Vol 7, Issue 20
Re: Al / 2% / Si MEMS-talk Digest, Vol 7, Issue 20
2003-05-16
[email protected]
Re: Al / 2% / Si MEMS-talk Digest, Vol 7, Issue 20
[email protected]
2003-05-16
Means Al with 2% Silicon - used to reduce junction spiking in contacts.


avi


Message: 10
Date: Fri, 16 May 2003 10:13:21 +0800
From: "bobo" 
Subject: [mems-talk] meaning of Al/2%/Si
To: 
Message-ID: <000701c31b50$bc5e0dc0$720110ac@cxm>
Content-Type: text/plain;            charset="gb2312"

hi,everyone, who knows the meaning of "Al/2%/Si"? Thanks a lot.





Avi Laker
Teccor Electronics
972 756 8237   Office
214 439 6770   Pager



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMS Technology Review