Hi All:

There is a recent paper by Karin Glasmastar from Chalmers University in
Sweeden that investigated this problem. It is published in one of the most
recent edition of Langmuir (it is still under the asap category).
They indeed found that there is a lot of silicone transfer whenever PDMS is
contacted to a surface. They suggest that a UV-ozone treatment reduced this
transfer. We found in our work that leaving the  PDMS overnight in ethanol
allowed the leach out of most of the unreacted monomers and oligomers. A
better way was to use a soxhlet extraction in ethanol too.
Karim


-----Original Message-----
From: Alik Widge [mailto:[email protected]]
Sent: Sunday, June 01, 2003 12:11 PM
To: General MEMS discussion
Subject: Re: [mems-talk] PDMS residue imprint


I recall seeing one paper where PDMS microstamps were extracted overnight
in chloroform to remove low molecular weight residues. I personally have
not had the problem you describe, so I've never tried the extraction. You
should expect, though, that it would cause swelling of your PDMS (as most
organic solvents do), so if the PDMS is adhered to something already, I
suspect it would delaminate due to the strain of the expansion.

Alik Widge
MEMS Laboratory
Carnegie Mellon University


--On Friday, May 30, 2003 4:02 PM -0500 Christopher Khoury
 wrote:

> Group,
>
> is anyone familiar with removing excess residues or uncured monomer from
> PDMS? A patterned imprint residue is highly noticable anytime PDMS comes
> in contact with glass in particular. Usually this imprint can be seen
> through side illumination or scattering off the glass.        So far I've
tried
> pulsed and unpulsed sonication of the PDMS mold in both water and dilute
> ethanol, this only seems to improve things marginally.
>
> Thanks,
>
> C. Khoury
>
>
> Christopher Khoury
> Microsystems Engineer
> Nanosphere, Inc.
> 1818 Skokie Blvd Suite 200
> Northbrook IL 60062
> 847-656-0240
>
> This transmission may contain confidential information which belongs to
> the sender. This information is intended only for the use of the
> individual or entity named above.  If you are not the intended
> recipient, you are hereby notified that any disclosure, reproduction, or
> distribution of this information, or any action taken in reliance on the
> contents of this information is strictly prohibited.  No confidentiality
> or privilege is waived or lost by any miss transmission.  If you have
> received this transmission in error, please notify us immediately at
> (847) 562-8880 and return the email to the sender by reply.
>
>



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Nano-Master, Inc.
Mentor Graphics Corporation