Foundry Services
2003-07-25
Omar Zohni
2003-07-28
Chris Kovach
Foundry Services
Chris Kovach
2003-07-28
Omar,

Can you be more specific on your requirements?

Chris

____________________________________________
Chris Kovach, Ph.D.
Executive Director
The Center for Micro and Nano Processing
The Microfabrication Laboratory
The Electronics Design Center

Case Western Reserve University
10900 Euclid Avenue
Bingham Building, Rm 107A
Cleveland, OH,  44106-7200

Ph: (216) 368-3628
Fax: (216) 368-8738
[email protected]




-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Omar Zohni
Sent: Friday, July 25, 2003 4:27 PM
To: General MEMS discussion
Subject: [mems-talk] Foundry Services


Hi Everyone:

I was wondering if anyone has some sources for a processed silicon wafer
that has a Nitride/Titanium/Platinum stack on the front side and a
Nitride deposition on the back.

Thanks
omar.



-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Rich Rosenblum
Sent: Friday, July 25, 2003 10:50 AM
To: [email protected]; General MEMS discussion
Subject: Re: [mems-talk] Desperately seeking MEMS videotape.


Joao,

Some of the material produced for www.semi.org that I viewed is very
compelling.  You can start with "Silicon Magic"

See  - http://dom.semi.org/webcatalog.nsf/itemList?OpenForm&group=1300


Regards,

Rich Rosenblum
Principal Electrical Engineer
Ametek PMT
[email protected]






"[email protected]" 
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review