MEMSnet Home: MEMS-Talk: Re: Diffusion or Ion implantation
Re: Diffusion or Ion implantation
2003-08-06
Tiansheng Zhou
2003-08-07
Chris Kovach
2003-08-06
[email protected]
2003-08-07
Karl Cazzini
2003-08-06
Maurice Norcott
2003-08-06
[email protected]
2003-08-07
Kim Norris
Re: Diffusion or Ion implantation
Maurice Norcott
2003-08-06
Try Core Systems in Santa Clara. CA for implants

Seaway in Livermore, CA might be able to do diffusion.
Noel in Campbell CA might be able to do diffusion also.


-----Original Message-----
From: Tiansheng Zhou [mailto:[email protected]]
Sent: Wednesday, August 06, 2003 11:45 AM
To: [email protected]
Subject: [mems-talk] Re: Diffusion or Ion implantation


Hi All:

I am looking for a vendor for diffusion or Ion implantation of 4"
silicon wafers.

Thanks for any lead information.

--
Tian


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering
Nano-Master, Inc.