Husein Rokadia
2003-08-14
Hey Guys,
I am trying to sonicate Multiwall Carbon Nantoubes in Isopropyl Alcohol.
My current mixing ratio is 1mg of CNT /100 ml of IPA for about 2 hours.
The problem with my current method is that the CNTs coagulate very quickly
after I stop the sonication, I have tried to sonicate for a longer duration
but to no avail.

I am wondering if there is a problem with my concentration ratio, or if I
should  switch to some other solvent?
Alternately please suggest sonication recipies of your own.

Thanking you in anticpation,

Sincerely,
Husein Rokadia

Husein Rokadia
University of Arkansas,
MEEG Rm 223,
O:479-575-6821
R:479-871-0033
Lab:479-575-4150


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMS Technology Review