Hello Everyone,

I am new to playing with SU-8. Rather than spin coat and process on silicon
I wish to replace the silicon wafer with a plastic substrate to which the
SU-8. Compatibility of the SU-8 with the plastic requires that:
1        The resist must adhere to the plastic
2      Solvent in SU-8  and developer must not swell or dissolve the plastic
3    Plastic should expand and contract isotropically during the baking and
cooling processes with a similar thermal expansion coefficient to the SU-8
(polymerised.

Does anyone out there have any suggestions about a suitable plastic ?
If you do and it is them my life gets easier.

Many thanks to you all.

Bob


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
University Wafer