Thermoplastic and photopatternable resin
2003-09-10
Paolo Bondavalli
2003-09-10
George D Gregoire
Thermoplastic and photopatternable resin
Paolo Bondavalli
2003-09-10
Hi all MEMS experts,
I'd like to know if a photopatternable and thermoplastic resin exists.
Bye.


*********************************************************
Dr. Paolo Bondavalli
R&D Engineer
MICROTEC MEMS
THALES (ex THOMSON-CSF) CORPORATE RESEARCH CENTER
Domaine de Corbeville,
Route Departementale 128
F91404 ORSAY
(FRANCE)
Tel : 01 69 33 08 63
Fax : 01 69 33 08 62
Email : [email protected]
**********************************************************
Disclaimer: Opinions expressed herein are my own and may
  not represent those of my employer.
**********************************************************



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics