MEMSnet Home: MEMS-Talk: Gold - Silicon Diffusion Coefficients (Au-Si)
Gold - Silicon Diffusion Coefficients (Au-Si)
2003-09-18
[email protected]
Gold - Silicon Diffusion Coefficients (Au-Si)
[email protected]
2003-09-18
I am looking for the diffusion coefficients for Gold in Silicon preferably over
temperature.  I have been unsuccessful in finding anything with a web search.
If anyone has a reference off the top of there heads it would be greatly
appreciated.

Ryan