Liwei Wang
2003-11-08
Eric Miller
2003-11-09
Shay Kaplan
2003-11-10
Ertl, Stephan
Magentic stir in KOH etching
Eric Miller
2003-11-08
You will find the stirring will help the temperature uniformity within the
bath to ensure you get a uniform etch.  You should also put a condenser/lid
over the bath to maintain the concentration of KOH is solution.

Eric Miller
----- Original Message -----
From: "Liwei Wang" 
To: 
Sent: Friday, November 07, 2003 2:18 PM
Subject: [mems-talk] Magentic stir in KOH etching


> Dear all:
>
> I am setting up a KOH etching station right now for deep etching Si
> (etch through the 500um wafer).I plan to have a constant temperature
> bath, a beaker, and a nice wafer holder to protect the backside of the
> film. my concern will be that do I need to have a magnetic stir set up
> in this KOH etching system? because it will be at least 10 hours
> etching, if so, how I gonna make it work? Put a magnetic plate in the
> water bath? or underneath the whole bath? does anyone have any
> experience or suggestions?
>
> Thank you so much in advance.
> Wish everybody have a nice weekend.
>
> Ivy
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing