wafers & thin films
2003-11-11
Jo-Ey (Joey) Wong
2003-11-12
Ravi Mullapudi
2003-11-12
Renie Duvall
wafers & thin films
Ravi Mullapudi
2003-11-12
Hi Jo-Ey,

Hionix (www.hionix.com) can certainly do the stack and provide you with the
wafers. Please let me know if your exact specifications and quantity.

If you need any further information please don't hesitate to call me at
408-910-8070.

Thanks
Ravi

-----Original Message-----
From: Jo-Ey (Joey) Wong [mailto:[email protected]]
Sent: Tuesday, November 11, 2003 1:14 PM
To: [email protected]
Subject: [mems-talk] wafers & thin films


Hi,

I am looking for vendors who could supply small
quantities of 4" wafers with film stack of 200 nm
thermal oxide, 250 nm of aluminum, and 1.5 um of
silicon.

    -----------
    1.5 um Si
    -----------
    250 nm Al
    -----------
    200 nm SiO2
    -----------
    4" Silicon
    Substrate
    -----------

Please email suggestions and comments to
"[email protected]". Thank you!

Jo-Ey Wong


---
Incoming mail is certified Virus Free.
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.536 / Virus Database: 331 - Release Date: 11/3/2003

---
Outgoing mail is certified Virus Free.
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.536 / Virus Database: 331 - Release Date: 11/3/2003


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Nano-Master, Inc.