MEMSnet Home: MEMS-Talk: Wafer temperature measurement
Wafer temperature measurement
1997-12-04
Greg White
Wafer temperature measurement
Greg White
1997-12-04
If it is OK to alter the emissivity of the wafer for your purposes,
paint it with manifold paint, bake it out, and use an IR camera to
determine temperatures (this doesn't work real well with product
wafers, but it's fine if you are looking for things like temperature
uniformity).  I have realtime video of a wafer undergoing (destructive)
thermal shock by this means.

-Greg


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
University Wafer
Process Variations in Microsystems Manufacturing