MEMSnet Home: MEMS-Talk: Stress relaxation in aluminum
Stress relaxation in aluminum
2003-12-10
Nadav Agian
Stress relaxation in aluminum
Nadav Agian
2003-12-10
Hey all,
What is the best procedure for stress relaxation of aluminum ( deposited on
Silicon)?
Nadav Agian

R&D Engineer

Remon Medical Tec. Ltd.

Tel: +972-4-623 00 01 ext. 148

Fax: +972-4-623 08 36