MEMSnet Home: MEMS-Talk: Aluminum evaporation or Aluminum sparker
Aluminum evaporation issues
2004-01-07
Sachin Rane
2004-01-07
Steven F. Nagle
2004-01-08
???
2004-01-13
David Grove
2004-01-08
[email protected]
2004-01-13
Sachin Rane
Aluminum evaporation or Aluminum sparker
2004-01-14
hengcw
2004-01-14
R. Brent Garber (2 parts)
2004-01-16
hengcw
Aluminum evaporation or Aluminum sparker
R. Brent Garber
2004-01-14
Heng,

I bought 2 BOC Edwards Auto 306 thermal evaporators.  The are fairly cheap but
small.  We have been happy with them for the most part.

Brent

hengcw wrote:

> Hi All,
>
> Can some body give me the information of company which manufacture aluminum
> evaporation or aluminum sparker machine for research purpose.  Thanks
>
> Heng
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
garber.vcf (text/x-vcard, 361 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Mentor Graphics Corporation
Harrick Plasma, Inc.