Rhodium plating
2004-01-19
Choe,S-H
BST thin film phase shifter
2004-01-19
Mr. Indrajit Paul
Rhodium plating
Choe,S-H
2004-01-19
Dear All;

Hello. I am now trying to electroplate Rhodium.
It is said that Rhodium is well suited for parts such as sliding electrical
contancts that require protection from corrosion, and it is the hardest
of all of the precious metals.

But, I could not find the plating solutions that are useful for
micromachining
I found that MIL-R-46085 shows the specification for the Rhodium plating.

If you have any information on Rhodium plating, please let me know that.

Thanks you all for helping me everytime.

Choe,Seong-Hun
Esashi Lab, Tohoku University, Japan
E-Mail: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing
MEMStaff Inc.