MEMSnet Home: MEMS-Talk: Help needed with solent semiconductor reflow oven
Help needed with solent semiconductor reflow oven
2004-02-05
[email protected]
Help needed with solent semiconductor reflow oven
[email protected]
2004-02-05
Hi all,

We purchased some time ago used reflow oven from auction at USA. Here is
picture from it:

http://www.orc.tut.fi/manual/reflow%202.jpg

Now we have problems using system because we don?t have manual and company
who made oven does not exist anymore. We would really appreciate any
contact information to someone who has this kind of system or other helpful
info. Please answer directly via mail.

Best regards,
Jukka Viheriala

Researcher,
Optoelectronics research center
Finland




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics