MEMSnet Home: MEMS-Talk: Details of chemically etching or electropolishing Ti and Ni based samples
Details of chemically etching or electropolishing Ti and Ni based samples
2004-02-17
ROBERT THOMPSON
Details of chemically etching or electropolishing Ti and Ni based samples
ROBERT THOMPSON
2004-02-17
I am considering chemically etching or electropolishing Ti and Ni based
tensile samples of thickness on the order of a millimeter from a bulk
sheet of Ti or Ni material.

Would the photoresist and/or mask solutions be similar to those listed on a TEM
website or are there other better options for the "machining" procedure that I
have in mind?  Any specific ideas?

Also, any comments on how the edge quality and shape accuracy would compare to
that of a sample made using a laser milling system or a micro EDM?  Currently,
mass
production of these tensile samples is not really an issue.

Thanks,
[email protected]




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
Addison Engineering