MEMSnet Home: MEMS-Talk: Electrodes on SU8 or PDMS
Electrodes on SU8 or PDMS
2004-02-26
NIU Xize
Electrodes on SU8 or PDMS
NIU Xize
2004-02-26
Dear all,

I'd like to deposit some electrodes on SU8 or PDMS layers, is it
possible? and the related process flow? Thanks!

Steven

reply