MEMSnet Home: MEMS-Talk: RIE of poly-Si on Si3N4
RIE of poly-Si on Si3N4
2004-03-03
Makuc, Boris
Parylene Data for thermomechanical simulation
2004-03-04
Erik Jung
2004-03-04
Michael D Martin
RIE of poly-Si on Si3N4
Michael D Martin
2004-03-04
Hi Boris,
   We have no problem stopping on LPCVD nitride (2 micron) for through
wafer etching (500 microns) with SF6 and O2 (~10%) in a STS ICP etcher.

-Mike


>>> [email protected] 3/3/2004 3:01:14 PM >>>
Hello all,

I need to etch ~7500A poly-Si patterned with S1813 resist and stop on
Si3N4.
The etch tool is a batch process, non-loadlocked, parallel plate design
with
13.5 MHz RF power to substrate electrode. Available process gases are
CF4,
CHF3, and O2. I may be able to substitute SF6 for CF4, but cannot use
Cl-based chemistries due to safety concerns.

The literature indicates that CF4-O2 chemistry produces highest Si etch
rate
at ~12% O2. I was thinking to run this mixture at low pressure and high
RF
power to obtain a fast Si etch and some sidewall taper (need good metal
step
coverage over the etched poly lines).

What is the typical Si/SiN selectivity under such conditions? Will
pressure/power significantly affect it? How does Si/SiN selectivity
vary
with %O2 in a CF4-O2 process? SF6 will increase etch rate and reduce
resist
loss, but are there other advantages to using it in this application?

I'd appreciate any recommendations and/or links to information. Thanks
a
lot.

Boris



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
University Wafer