lgovinda
UV curable adhesive
lgovinda
2004-04-12
Hi , my name is abhiram, could some one let me know if there is a UV
curable adhesive for SU8 spesimen to be bonded to a metal,say aluminum.i
contacted quite a few companies, but unfortunately none of them are
aware about SU8.i told them that it is an epoxy material.if some one is
aware of this, i would like to know whom to contact to get further
information about the same.i want to bind the SU8 to an aluminum piece.

thanking you.

regards
abhiram.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
MEMS Technology Review