Si surface roughness in DRIE process
2004-05-27
Qing Yao
2004-05-27
Ariel Lipson (IC)
2004-05-28
Kirt Williams
2004-05-28
Sunny Kedia
Si surface roughness in DRIE process
Sunny Kedia
2004-05-28
Qing Yao,

An EPW etch ( Ethylenediamine pyrocatechol and water) can be done to improve
the surface roughness, There is a paper "Anisotropic Si Etching Technique
for optically smooth surfaces" by Sasaki Metal in Eurosensors xv.

Sunny Kedia



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
Mentor Graphics Corporation