two options:
1. use of vitreous carbon crucible liner or
2. no use of any crucible liner, just place Pt start source directly on Cu
hearth.
Hope it helps
========================================
Honggang Jiang,
Materials Science Engineer
Second Sight
12744 San Fernando Road
Building 3
Sylmar, CA  91342
Ph: 818 833 5058
Fx: 818 833 5067
========================================

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of
abhishek jain
Sent: Thursday, June 03, 2004 8:16 PM
To: [email protected]
Subject: [mems-talk] Query


Hi,

Can anyone tell me what is the crucible that can be used for Platinum in
ebeam.

Thanks.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Nano-Master, Inc.
MEMS Technology Review