protection for KOH etch
2004-06-08
Isa Kiyat
protection for KOH etch
Isa Kiyat
2004-06-08
I always etch two silicon wafers or chips sticked to each other, from front
sides using some black-wax. This process both protects front sides and let
you etch two wafers at the same time. Also one wafer can be handle if you
want. I succeeded to fabricate two 4 um thick diaphragms at the same time
with this process.

===================================

Isa Kiyat

Bilkent University
Department of Physics
06800
Ankara, Turkey





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.