MEMSnet Home: MEMS-Talk: Drilling holes in Si
Drilling holes in Si
1998-11-30
Kirthi Roberts
Drilling holes in Si
Kirthi Roberts
1998-11-30
Dear MEMS enthusiasts,

Has anyone laser drilled holes on a 50-100
micrometer thick silicon membrane, to get a roughly
cylindrical cavity. I need holes of diameter of
about 50 micrometers on a Silicon membrane of the
above mentioned thickness. If anyone knows of any
publications in this area or can offer any advice or
tips, I would much appreciate if you could send them
to me.

Thanks in advance,

Kirthi Roberts

--
__________________________________
Kirthi Roberts
School of Engineering Science
Simon Fraser University
Vancouver,
Canada
e-mail : [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Tanner EDA by Mentor Graphics