MEMSnet Home: MEMS-Talk: Regd KOH setup
Regd KOH setup
2004-06-28
Dhanamjaya R Guda
Regd KOH setup
Dhanamjaya R Guda
2004-06-28
Hi All,

     I want to make a permanent set up for etching of silicon using KOH
etchant. I would like to see how the set up would look like. If any one has
any pictures, I would be very glad to have a look at them.

Thanks,
Dhanamjaya Reddy Guda