MEMSnet Home: MEMS-Talk: KOH etching protection
KOH etching protection
2004-06-05
Li Wang
2004-06-06
Jed Ley
2004-06-07
Rick Morrison
2004-06-08
Jan Lichtenberg
2004-06-14
taya sunil
2004-06-29
Regina Mueller
KOH etching protection
Regina Mueller
2004-06-29
Dear Li Wang,
we are able to solve your problem with our silicet vacuum wafer-holders. For
first information please see our website www.silicet.de. Feel free to
contact us directly.

Best regards
Regina Müller

silicet AG
Lindenbergstr. 30
D-34253 Lohfelden
fon: +49 (0) 0561-51 09 02 60
fax: +49 (0) 0561-51 81 66
mail: [email protected]
internet: www.silicet.de


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics