MEMSnet Home: MEMS-Talk: Palladium
Palladium
2004-07-07
Tripp, Marie Kathleen
2004-07-07
Christopher Blanford
2004-07-09
Pfoertner, Hugo
Palladium
Christopher Blanford
2004-07-07
Dear Marie

For Pd on its own, these values are listed on webelements


Young's modulus: 121 GPa
Rigidity modulus: 44 GPa
Bulk modulus: 180 GPa
Poissons ratio: 0.39
Mineral hardness: 4.75
Brinell hardness: 37.3 MN/m2
Vickers hardness: 461 MN/n2
Electrical resistivity: 10 W m
Thermal conductivity: 72 W/m/K
Coefficient of linear thermal expansion: 11.8 ppm/K

Chris

On Wednesday, July 7, 2004, at 04:47 PM, Tripp, Marie Kathleen wrote:

> Can anyone recommend a good reference for mechanical properties (
> young's modulus, poisson's ratio, coefficient of thermal expansion)
> for  Palladium and/or alloyed Gold-Palladium (60:40)?    Thanks, Marie

--
Christopher F. Blanford
Inorganic Chemistry Laboratory, South Parks Road, Oxford, OX1 3QR, UK
Phone: +44 (0)1865 282603; Fax: +44 (0)1865 272690
PGP keyID: 8D830BC9  http://pgp.mit.edu/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Addison Engineering
Mentor Graphics Corporation